Difference between revisions of "Visual inspection"
From GlueXWiki
(→Possible issues with lead glass module) |
(→Possible issues with lead glass module) |
||
Line 23: | Line 23: | ||
#* lead glass module has to be disassembled; the glass block has to be replaced. | #* lead glass module has to be disassembled; the glass block has to be replaced. | ||
# Issues with wrapping | # Issues with wrapping | ||
− | #* small damages (holes) | + | #* small damages (holes) in the Aluminized mylar, see Fig. 2. This can be fixed by using Al sticky tape, thickness < 20 um |
− | #* | + | #* Aluminum layer in the wrapping foil peels off or adheres to the glass block (penetrates into the block): |
− | #** | + | #** Fig. 3 and Fig. 4: Aluminum layer peeled off resulting in some transparent holes in wrapping. |
+ | #** Recommend to disassemble and re-wrap the lead glass block |
Revision as of 11:02, 18 October 2022
Possible issues with lead glass module
- Broken lead glass, see Fig. 1 (module taken from the FCAL prototype)
- some problems can be seen by looking on the lead glass block from the side opposite to the PMT
- lead glass module has to be disassembled; the glass block has to be replaced.
- Issues with wrapping
- small damages (holes) in the Aluminized mylar, see Fig. 2. This can be fixed by using Al sticky tape, thickness < 20 um
- Aluminum layer in the wrapping foil peels off or adheres to the glass block (penetrates into the block):
- Fig. 3 and Fig. 4: Aluminum layer peeled off resulting in some transparent holes in wrapping.
- Recommend to disassemble and re-wrap the lead glass block