Difference between revisions of "Visual inspection"
From GlueXWiki
(→Possible issued with lead glass module) |
|||
Line 15: | Line 15: | ||
</gallery> | </gallery> | ||
− | == Possible | + | |
+ | == Possible issues with lead glass module == | ||
# Broken lead glass, see Fig. 1 (module taken from the FCAL prototype) | # Broken lead glass, see Fig. 1 (module taken from the FCAL prototype) | ||
− | #* some problems can be seen | + | #* some problems can be seen by looking on the lead glass block from the side opposite to the PMT |
#* lead glass module has to be disassembled | #* lead glass module has to be disassembled | ||
# Issues with wrapping | # Issues with wrapping | ||
#* small damages (holes) of the Aluminized mylar, See Fig. 2. Can be fixed using Al sticky tape, thickness < 20 um | #* small damages (holes) of the Aluminized mylar, See Fig. 2. Can be fixed using Al sticky tape, thickness < 20 um | ||
− | #* | + | #* Al layer in the wrapping foil peels off or adheres to the glass block (penetrates into the block): |
#** Al layer peeled off resulting in some transparent holes in the wrapping. | #** Al layer peeled off resulting in some transparent holes in the wrapping. |
Revision as of 10:54, 18 October 2022
Possible issues with lead glass module
- Broken lead glass, see Fig. 1 (module taken from the FCAL prototype)
- some problems can be seen by looking on the lead glass block from the side opposite to the PMT
- lead glass module has to be disassembled
- Issues with wrapping
- small damages (holes) of the Aluminized mylar, See Fig. 2. Can be fixed using Al sticky tape, thickness < 20 um
- Al layer in the wrapping foil peels off or adheres to the glass block (penetrates into the block):
- Al layer peeled off resulting in some transparent holes in the wrapping.